Post time: 06-03-23The external environment has great influence on the preservation of galvanized wire mesh. In the rainy season, it is necessary to pay attention to the air humidity of the workshop, warehouse and other departments. It is recommended to use a humidifier. Usually, the moisture absorption of book paper is larger than that of powder paper, and the pH value is higher. Generally speaking, in the normal environment of storage wire, storage time of two years is not corroded wire phenomenon. However, it should be noted that in the process of handling the iron wire, it should be handled gently to avoid the position of the coiling coil, which will cause the smooth pulling of the wire and affect the production.
- 5, after the light plating should be carried out light treatment.
Post time: 22-09-22Environmental factors should be considered when choosing the thickness of galvanized layer. Galvanized wire in galvanized, pay attention to the above problems, can be well galvanized, to ensure the quality of galvanized wire. Galvanized methods are mainly divided into two types, one is hot dip galvanizing method, the other is electric galvanizing method. This paper mainly introduces the method of galvanizing. Electrogalvanizing is an electrolyte used for galvanizing.
Post time: 20-06-22- Arrived in other ways can’t end effect of the inclination of hook flower network structure in essence is void, water permeability, the natural effect of groundwater and filtering effect has a strong inclusive, suspended in the water content and silt accumulation in fill in crevices, applied to mountain protection, is conducive to the growth of natural plant, beautify the grass spraying to arrive late his curing effect, Gradually restoring the original ecological environment is a perfect connection between beautification and protection.
1, stress relief before plating where the maximum tensile strength is greater than 1034Mpa key and important parts before plating should be at 200±10℃ stress relief for more than 1 hours, carburizing or surface quenching parts should be at 140±10℃ stress relief for more than 5 hours.
Steel mesh jinsu appearance treatment: polyethylene thermoplastic powder coatings is also called polyethylene powder coating, is the high pressure polyethylene (LDPE) as the basic material, adding a variety of function additives, colors, its antiseptic powder coating manufacturing processes, jinsu coating layer has the function of chemical, shock, circuitous, acid, salt fog corrosion, decorate a function and has good appearance.
Post time: 12-01-23- 3, look at the packaging, the normal packaging appearance is to use a layer of kraft paper paper with film to package our welded welding net, so that it will not be oxidized and rusted in transit.
- In general, the organic matter contained in the galvanized wire can make the plating speed significantly reduced. Although the chemical formulation is conducive to high deposition rate, but the organic matter with the coating thickness can not meet the requirements, so activated carbon can be used to treat the tank liquid. Zinc is a silver-white metal, brittle at room temperature, soluble in acid can also be soluble in alkali, known as amphoteric metal.
Post time: 21-09-22Paint on the galvanized layer, the binding force between each other and the baking temperature of the paint has a great relationship, after galvanized coating alkyd paint, adhesion is no problem. Galvanized amino paint, paint adhesion is not good. Do two bottom two surface, adhesion is ok, if the two bottom two surface to two bottom three surface, that is, more paint, more baking once, again test adhesion is very poor, poor to the paint from the galvanized layer of pieces torn off.
- 5. Dry it with a towel.
- Hook mesh from the point of view of weaving quality inspection requirements, hook mesh wire and silk staggered can not loose, the whole piece of hook mesh can not loose deformation. Of course, if the customer special requirements out of the net, showing loose phenomenon can not blame the production side. Whether the mesh meets the specification requirements and the wire diameter meets the wire diameter.
Post time: 24-10-22- Specifications: Complete (m)
A variety of arc, undivided Angle and undivided elevation ladder mounts are available to provide the ideal treatment plan. It can be used together with the appearance and the design of the common trackless active shift door, forming a harmonious and intact whole.
Iron has gray iron, white iron and the above – mentioned combination of gold, each of which has different characteristics, so in industry, according to their different characteristics to transport and selection. For example, in gray iron, its carbon exists in iron ore as graphite, and the crack is often gray, soft and tough, simple filter cutting, which is suitable for casting.
Post time: 29-05-23The main raw material of blade barbed rope is galvanized wire and galvanized sheet, because the price of galvanized sheet is more expensive than galvanized wire, so it is directly reflected in the price of the sales of blade barbed rope. There is also the difference in processing technology also led to the difference in the price of the blade thorn rope. The traditional barbed rope is mechanically twisted, which uses less labor and has high production efficiency. But the blade is after two mechanical processing in the manual processing operation before the appearance. So whether from the labor force or from the production efficiency also said there is a large gap. These factors lead to the price of blade thorn rope is more expensive the main factor.
- Avoid hanging cages near heaters, as failure to dissipate heat can interfere with bird molting.
The methods to control the thickness of galvanizing are as follows: you can slow down the lifting speed of the workpiece, control the time of galvanizing as far as possible, add the appropriate amount of thinning alloy, reduce the thickness, and improve the temperature of hot-dip galvanizing. But consider the zinc pot, iron pot should not exceed 480 degrees, ceramic pot can be 530 degrees, which can reduce the time of zinc immersion.
There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.